DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature (Tg), melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).

SKZ Industrial 550°C DSC OIT tester delivers ±0.1°C temp repeatability & 0.01μW DSC resolution. Cuts oxidation stability testing time by 35%. Trusted by 200+ labs; ISO/IEC 17025-compliant. Request ROI Analysis Report.
Product Description

Technical parameters:

Temperature range

RT~ 550 ℃

Heating rate

0.1~80℃/min

Temperature resolution

0.001℃

Temperature fluctuations

±0.001℃

Temperature repeatability

±0.1℃

Constant temperature time

Program setting ≤24h

SKZ Industrial Co., Limited

D-11, No.9 Lanxiang road, Tianqiao District, Jinan, Shandong province, China.

Tel: +86-531-68825087, 0086-15692312640

Web: www.skzindustrial.com

DSC range

0~±600mW

DSC noise

0.01μW

DSC resolution

0.01μW

DSC accuracy

0.01mW

Atmosphere control gas

Nitrogen, Oxygen (instrument switch automatically)

Gas flow rate

0-300mL/min

Gas pressure

0.2MPa

Control Mode

Rising temperature, constant temperature(full automatic)

Curve scanning

Rising scan

Gas flow control

Built-in digital flow meter & Software control, automatic

Display

24 bit 7 inches LCD touch screen display

Data interface

standard USB connector

Parameter standard

With standard material, with calibration function, the user may correct temperature and heat enthalpy

Software

operating software

Thermocouples

Total 3 sets of thermocouples for:

1). Test sample temperature

2). test furnace temperature,

3). Test internal ambient temperature

Cooling device

Air cool

Power

AC220V/50Hz

Packing List

Host instrument

1PC

CD

1PC

Data Line

1PC

Power Line

1PC

Aluminum crucibles

100PCS

Ceramic crucibles

100PCS

pure tin grains

1bag

Fuse 4A

5PCS

DSC is designed to determine the inner heat transition relating to temperature and heat flow, it is widely used in the field of polymer development, performance testing & quality control. DSC research and development includes the following field: glass transition temperature (Tg), melting point, cold crystallization, crystallization, phase transition, oxidation induction time (OIT).

Contact Us

Name
Email
Whatsapp / Mobile
What would you like to inquire about
Message
0/1000

Standards

ISO/TR10837: 1991, ASTM D3895-1998, ASTM E 967, ASTM E 968, ASTM E 793,AST M D 3895, ASTM D 3417,ASTM D 3418, ISO 11357-6

SKZ1052 Product Advantages

Ⅰ

Ⅰ

The industrial-grade 7-inch touch screen displays rich information.
Ⅲ

Ⅲ

USB communication interface, strong versatility, reliable and uninterrupted communication, supports self-recovery connection function.
Ⅴ

Ⅴ

The software is simple and easy to operate.
product
Ⅱ

Ⅱ

Brand-new metal furnace body structure, with better baseline and higher accuracy. The heating adopts the indirect conduction method, which has high uniformity and stability, reduces pulse radiation, and is better than the traditional heating mode.
Ⅳ

Ⅳ

Automatically switch the two-channel atmosphere flow, fast switching speed and short stabilization time. At the same time, a protective gas input is added.

Product Certification

With 17 years of expertise, we deliver certified quality you can trust.
Get a Quote
Product Certification

Get a Free Quote

Our representative will contact you soon.
Name
Company Name
Email
Whatsapp / Mobile
Message
0/1000

SKZ1052

PRODUCT DETAILS

USB Communication Interface

Strong versatility, reliability, and uninterrupted communication support the self-recovery connection function.

USB Communication Interface

U-shaped Furnace Body

Metal U-shaped furnace body has good repeatability. Anodic oxidation processing is more corrosion-resistant.

U-shaped Furnace Body

Sensor

The heating adopts the indirect conduction method, which has high uniformity and stability, reduces pulse radiation, and is better than the traditional heating mode.

Sensor

Application of Differential Scanning Calorimeter

  • Organic matter
  • Inorganic matter
  • Polymers
  • Metals
  • Semiconductors
  • Medicines
  • Biomaterials
LEARN MORE
  • laboratory fully automatic 550c differential scanning calorimeter dsc oxidation induction time oit oxidation stability determination equipment tester-0
  • laboratory fully automatic 550c differential scanning calorimeter dsc oxidation induction time oit oxidation stability determination equipment tester-1

Shipment

Shipment and Delivery

365-Day One-Stop Service

Shipment and Delivery

Alibaba's top certified supplier provides a one-to-one logistics tracking reminder service.

 What about the transportation?
What about the transportation?

1000

Satisfied clients

Shipment and Delivery
  • Provide air, sea and shipping services according to customer needs

  • Provide fumigation-free plywood boxes or multi-layer cartons, wrapped with plastic film inside

  • Delivery within two weeks

  • Low minimum order quantity OEM

24/7 Support
24/7 Support

See How Our Instruments Work

This video lets you learn more about the product's advantages, applications, and testing details.

Usage Tutorial

Usage Tutorial

Operation Demonstration

Operation Demonstration

inquiry

Contact Us

Name
Email
Whatsapp / Mobile
What would you like to inquire about
Message
0/1000
Recommended Products
laboratory fully automatic 550c differential scanning calorimeter dsc oxidation induction time oit oxidation stability determination equipment tester-2
laboratory fully automatic 550c differential scanning calorimeter dsc oxidation induction time oit oxidation stability determination equipment tester-3

Get a Free Quote

Our representative will contact you soon.
Name
Company Name
Email
Whatsapp / Mobile
Message
0/1000